Welding Tips And Tricks
RSS-
-
WM Blitz Video #12 115 Volt MIG 2F Corner Joint - PrimeWeld MIG180
Read nowMaterial type and thickness was 1018 steel 11ga .120" (3mm) 18.1 volts 149ipm using .035" ER70S6 wire, C25 gas at 25cfh This is a 2f position horizontal corner joint. It is only slightly different than a 1F flat position and...
-
WM Blitz Video #11 115 Volt MIG 11GA 3f Outside Corner Downhill MIG180
Read nowMaterial type and thickness was 1018 steel 11ga .120" (3mm) 18.1 volts 149ipm using .035" ER70S6 wire, C25 gas at 25cfh There are times when mig welding downhill makes sense and there are also times when uphill is called for....
-
WM Blitz Video #10 115 volt MIG Welder 11GA Outside Corner Joint - 1F Flat MIG180
An outside corner joint is a very common joint for fabricating tanks and reservoirs and this is the first of several quick videos showing techniques and settings.
-
WM BLITZ VIDEO #9 MIG Welding Overhead PrimeWeld MIG180 on 115volt
A long stickout reduces amperage and softens the arc and while you might see the puddle better, the weld often piles up.
-
WM Blitz Video #8 TIG Welding Aluminum 5F Weld Test - Tube to Plate 🔥
This 5f test is a fillet weld test that Andrew Cardin needed to pass in order to make a single aluminum socket weld on a Liquid Natural Gas (LNG) facility.