WM BLITZ VIDEO #9 MIG Welding Overhead PrimeWeld MIG180 on 115volt
A long stickout reduces amperage and softens the arc and while you might see the puddle better, the weld often piles up.
A long stickout reduces amperage and softens the arc and while you might see the puddle better, the weld often piles up.
This 5f test is a fillet weld test that Andrew Cardin needed to pass in order to make a single aluminum socket weld on a Liquid Natural Gas (LNG) facility.
In this video, I started out using a flow rate that usually works fine with a #7 gas lens cup.
My good friend Andrew Cardin came for a visit and we filmed a few videos.
This is one of them.
Textbooks will tell you that you must use a stainless steel wire brush on aluminum before tig welding. Is that really true? In my own experience, the way I clean aluminum depends completely on the situation. For sheet metal...