TIG Welding a Stainless Liquid Nitrogen Header

For this Video, I was at JD's shop working on a stainless steel liquid nitrogen header.

The header was made from  2" schedule 10 stainless with 2 end caps and 4 threaded o lets.

Before welding, we purged the line with argon using a Dual Flowmeter (click here to see the flowmeter on the store)

Using the Furick jazzy 10 ceramic and 20cfh flow of argon with 10 cfh purge, the root pass on the end cap butt joints were welded with 65-70 amps without filler metal.

After cooling and wire brushing with a stainless brush, a cover pass was done at roughly 65-70 amps.

A TIG Finger gives you a lot of options and a way to prop right next to the weld 

 

Artículo anterior Weldmonger Customer Quick Tip Video #4 Stick Welding with TIG torch

Comentarios

nathan - diciembre 4, 2024

as a newbie to crypto i lost alot of money, I would like to express my gratitude to Expert Bernie Doran for their exceptional assistance in recovering my funds from a forex broker. Their expertise and professionalism in navigating the complex process were truly commendable. Through their guidance and relentless efforts, I was able to successfully retrieve my funds of $150,000 providing me with much-needed relief. I highly recommend him on Gmail Berniedoransignals@gmail.com or whatsApp + 1 424 285 0682 to anyone facing similar challenges, as their dedication and commitment to helping clients are truly impressive. Thank you, Bernie doran, for your invaluable support in resolving this matter

Dejar un comentario

* Campos requeridos

Powered by Top Rated Local® RETURN TO TOP